(1)已完成的屋頂涂膜防水層應(yīng)采取保護(hù)措施,以免被其他操作工序破壞。應(yīng)在垂直墻面的屋頂涂膜防水層完成后立即鋪設(shè)保護(hù)材料;對于需進(jìn)行閉水試驗的部位,應(yīng)在閉水試驗完成并檢查無滲漏情況后,再鋪設(shè)保護(hù)層。若閉水試驗推遲則應(yīng)采取一些保護(hù)措施。
(1) protective measures to be done to prevent the coating from being damaged by other operating procedures. Should be in the vertical wall coating waterproof layer immediately after the completion of the laying of protective materials; for the need to carry out the closed water test site, should be completed in the closed water test and check the absence of leakage, and then laying protective layer. Temporary protection measures shall be adopted if the closed water test is postponed.
(2)地下工程:在垂直墻面上采用聚乙烯泡沫塑料片材做保護(hù)層時,可在最后一道涂膜固化前,直接黏貼5~6mm厚的發(fā)泡聚乙烯片材保護(hù)層(四川人事考試中心),并要求拼縫精密,然后按要求回填土;對平面部位的涂膜外觀,可干鋪一層紙?zhí)r青油氈作保護(hù)隔離層,并在其上澆注400mm厚細(xì)石混凝土作剛性保護(hù)層。
(2): underground engineering on the vertical wall surface using polyethylene foam sheet as a protective layer, but at the end of a film before curing, directly paste 5~6mm thick polyethylene foam sheet protective layer, and then according to the requirements of the joint close, backfill; coated surface of the planar parts, can be laying a layer of paper tire asphalt as protective isolation layer, and the thickness of 400mm fine stone concrete pouring for rigid protective layer.
(3)廁浴間地面及立墻保護(hù)層:可在涂膜厚度達(dá)到規(guī)定要求并經(jīng)驗收合格后(濰坊網(wǎng)絡(luò)公司),在涂膜外觀再涂一道涂料,并立即撒布少量干凈干燥的砂子,使其與涂膜屋頂防水層黏結(jié)牢固后(河南人事考試網(wǎng)),再涂抹水泥砂漿保護(hù)層。
(3) toilet ground and wall protection layer: in the film thickness to meet the requirements of the acceptance, in the film surface and then coated with a coating, and immediately spreading a small amount of dry sand, and the coating waterproof layer bonded firmly, then apply the protective layer of cement mortar.
(4)屋面屋頂防水層保護(hù):當(dāng)涂膜厚度達(dá)到要求并驗收合格后可在涂膜外觀上鋪紙?zhí)r青油氈或麻刀灰隔離層,再澆注細(xì)石混凝土剛性保護(hù)層。如需進(jìn)行閉水試驗,則保護(hù)層應(yīng)在閉水試驗后進(jìn)行鋪設(shè)。
(4) the roof waterproof protection: when the film thickness to meet the requirements and acceptance after the fetal asphalt felt paper or knife grey isolating layer on the film surface covered, then fine stone concrete pouring rigid protective layer. If the closed water test is required, the protective layer shall be laid after the closed water test.
(5)閉水試驗:對于屋面、廁浴間涂膜防水層有閉水試驗的要求時,可在涂膜屋頂防水層固化成膜36h之后,堵塞排水孔,進(jìn)行閉水試驗。
(5) closed water test: for the roof, toilet bath coating waterproof layer has closed water test requirements, can be in the film waterproof layer after curing film 36h, blocking the drainage hole, closed water test.